How was it tested?Hey Guys,
Where in the world can I sell arsenic ore (30%) I have tonnes or the stuff. Some samples have also shown PGMs along with it (Rh, Pd, Pt, Os, Ir. Au). Any guidance in this area will be very helpful.
ICP ... and we have tested with many labs. We were testing for PGM where sometimes PGM would show up in high PPM (>150) and some times very low (<15) but arsenic is always there at high percentage (>30%)How was it tested?
I doubt if this is saleable due to the Arsenic.ICP ... and we have tested with many labs. We were testing for PGM where sometimes PGM would show up in high PPM (>150) and some times very low (<15) but arsenic is always there at high percentage (>30%)
You are right to some extent, as it is proving to be difficult to sell as PGM Ore, hence I'm trying to see if I can sell it as Arsenic (due to the high content).I doubt if this is saleable due to the Arsenic.
I might be wrong though.
Enter your email address to join: