4metals said:What process did you use to solvate the gold? ...
Topher_osAUrus said:4metals said:What process did you use to solvate the gold? ...
I understand that gold in solution can form complexes, but, can you elaborate on how this one in particular comes about?
For instance, is this something that is common place to happen when doing regular gold processes (AR, is my main concern.-Im assuming it isn't). And, does this complex sodium-gold salt have problems precipitating out of solution with standard methods?(similar to how we should keep ammonia out of our processes, especially with pgm's, as they form a complex that even zinc has trouble reducing)?
How do they make this complex on a grand scale?
How might we accidentally make it?
I skimmed through my books, but they were not very forthcoming with pertinent information.
Truly and Honestly, it is better to follow a Known-To-Work process than throwing in many reagents and hoping for the best.bastinado said:... and bleach ?( 5% Naoh + 5% Naocl ) and then ... some of SMB ... add some of H2O2 , then some of sodium thiosulfate ...
Topher_osAUrus said:So, simply adding salt to an AR dissolve of gold will complex it to NaAuCl3?
In that case, what does the gold complex end up being when dissolving gold with bleach and hcl? And it is creating salt in the reaction, which would have sodium ions floating around in it, right?
And, what if a guy starts off with bleach+HCl and realises its too slow for thick foils, then adds a few mL's of nitric?
Unfortunately the Chemistry is quite complicated, which is why Hoke's instructions are a work of sheer Genius - she knew loads about the specific details, then wrote a book that made it easy for non-chemists to do.Topher_osAUrus said:I got a little more confused than clarified after those replies
I disagree, incinerate a gold chloride solution would lead to losses of volatile gold chloride.bastinado said:i think the best thing to do is to dry the solutions totally and then incinerate the salts
and re dissolve first in water
and the remain i would dissolve with acid and bleach but in moderate quantities