crgoode said:
Thanks for all the info guys. I am still a little worried about precipitating with Tungsten in the solution. I have sifted through so much information on this and am still getting conflicting outcomes. I will give it a try and see what happens.

Do a search on using copperas for doing your first drop of your gold, and then refine the recovered material again and use SMB for dropping your gold on the 2nd go round and you will be ok.
 
Thanks everyone for the input. I figured that, just for the heck of it, I would post the results:

After all was said and done, I got 0.74g of gold out of the first drop from two processors.

The tungsten that was present in the solution did not end up being an issue and was nothing that a little bit of HCL couldnt handle.

Thanks again everyone for your input
 