M MotoLupe New member Joined Jun 5, 2011 Messages 1 Jun 14, 2011 #1 I am having trouble with Butyl Diglyme dropping contents on wash cycle. I use HCL-CL method on gold ore and Butyl Diglyme will pick up yellow material and will pick up multiple shots of material but dumps it on the first wash.
I am having trouble with Butyl Diglyme dropping contents on wash cycle. I use HCL-CL method on gold ore and Butyl Diglyme will pick up yellow material and will pick up multiple shots of material but dumps it on the first wash.
Noxx Well-known member Joined Feb 24, 2007 Messages 3,365 Location Quebec, Canada Jun 16, 2011 #2 You're washing it with what and how does it precipitate ? Can you include a pic ?