can i use nano3 instead of nitric acid in ar?we are having dificulties in obtaining nitric acid here in Brasil. How can i dissolve scrap containing gold as quickly as i do with Ar?Any ideas?thanks for replies.
Thanks Dave,i looked for poors man Ar and know i have an idea how to proceed--Arthur, NaNO3 or KNO3 combined with HCl creates poor man's AR. You can search for that term for more details.
Dave
Yes it works good.Thanks Dave,i looked for poors man Ar and know i have an idea how to proceed--