Midlands
Member
I'm on good terms with the guy who operates my somewhat nearby refinery. I've always suspected they may pinch a little, but if so, it's probably just a little. Moreover, when my packages go to their other locations (for aquia regia process to remove diamonds or when I mail it in) every karat bag comes up noticably short in purity. I need an XRF so I can melt my scrap into a cake and XRF it before sending it in.
But I see websites with $12K XRF and others with $2k models.
Are there decent budget models I can use for gold and silver?
Are there good sources for used and remanufactured guns?
And are there models and sources I should avoid?
You guys are the only ones in the universe to ask this as a group. So please guide me with your collective wisdom.
Thanks!
But I see websites with $12K XRF and others with $2k models.
Are there decent budget models I can use for gold and silver?
Are there good sources for used and remanufactured guns?
And are there models and sources I should avoid?
You guys are the only ones in the universe to ask this as a group. So please guide me with your collective wisdom.
Thanks!