Electrochemistry Can only get coral like silver crystals

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.
If my goal was big crystals, I would look at the plating industry, and how they run their cells, and what they add to the electrolyte such as levelers or conditioners...

Searching through some of GSP's older posts would also be helpful I am sure, as he spoke so much of his work in the industry.
 
kurtak said:
For what it is worth I am a pyro at heart & one of my hobbies (besides refining) is making my own fireworks including making the explosive compounds to make the fireworks :shock: :mrgreen: :twisted:

Kurt, it must be a hell of fun having you as a friend.

I think that I still have a lot to learn and improve with the basic parameters before adding additives and complicating the matter even more.

I'm still looking for a large container