has anyone tried carbonated water to disolve lead ?
i just read that it will to some degree.it didnt say to what degree that was.
has anyone tried carbonated water if so how effective was it, or even if it was at all ?
 
When you add CO2 to water, you make Carbonic Acid (H2CO3).

It's a really weak acid and you'll only be able to dissolve PPMs of lead...
 