aflacglobal
Well-known member
This is a request from a possible customer of mine. The guys talking greek to me when it come to this. I am going to PM platinummills and ask for his soultion. That's a lot of material there. :shock: :shock: :shock:
wonder where it all goes. :lol:
Any idea's on the most productive and safe way for this to happen. I hate to kick him to the curb. He was reffered to me by a previous customer. You know how that buddy buddy system works.
Hi Mr Mattes
Thank you for your response, actually our company collect 10 tn of Auto Catalityc converter and smelt for recovery the PGM in Iron Matte Using a Electric Arc Furnace. This matte is refine in Jhonson Mattey ( Bet he's getting gouged ). We want to refine the PGM here in our plant in Bogota Colombia.
I know that we can disolve the PGM in Agua Regia directly from the Catalyst material but we need process 500 kg per days and are so dificult the disolution dimension and the filtration of this solid. We make somo proof of this method and need 12 hr almost for disolve the 90% of PGM present in the material and we need almost 98% of the recovery. And the other problem is the filtration size becuse we have 500kg of solid with 0.015% of PGM. If you have some solution for a directly digestion with high recovery results and fast filtration plese let me know. (Is so important the Rhodium recovery becouse is the 35% of the value of our material).
Any help ????
wonder where it all goes. :lol:
Any idea's on the most productive and safe way for this to happen. I hate to kick him to the curb. He was reffered to me by a previous customer. You know how that buddy buddy system works.
Hi Mr Mattes
Thank you for your response, actually our company collect 10 tn of Auto Catalityc converter and smelt for recovery the PGM in Iron Matte Using a Electric Arc Furnace. This matte is refine in Jhonson Mattey ( Bet he's getting gouged ). We want to refine the PGM here in our plant in Bogota Colombia.
I know that we can disolve the PGM in Agua Regia directly from the Catalyst material but we need process 500 kg per days and are so dificult the disolution dimension and the filtration of this solid. We make somo proof of this method and need 12 hr almost for disolve the 90% of PGM present in the material and we need almost 98% of the recovery. And the other problem is the filtration size becuse we have 500kg of solid with 0.015% of PGM. If you have some solution for a directly digestion with high recovery results and fast filtration plese let me know. (Is so important the Rhodium recovery becouse is the 35% of the value of our material).
Any help ????