• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Cementing out gold and forgot

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

chrundle_the_great

Well-known member
Joined
Dec 7, 2022
Messages
45
Location
Minnesota
Was cementing out some gold with copper and forgot about it, amd a bunch of copper sulfate? Chloride? Crystals formed. I can't remember for the life of me what it is called
 

Attachments

  • 20250129_145021.jpg
    20250129_145021.jpg
    2.1 MB
Was cementing out some gold with copper and forgot about it, amd a bunch of copper sulfate? Chloride? Crystals formed. I can't remember for the life of me what it is called
Most likely Copper Chloride as you used HCl and oxidizer to dissolve it.
Sulfate will only be if Copper dissolved in Sulfuric acid dried out, and that is quite blue.
 
Copper 2 chloride is soluble in water, so add hot water and dissolve what you can, what remains will be copper 1 chloride which is soluble in Hydrochloric Acid. What is left should be what you cemented. Just to be safe, check the liquids with stannous before calling them waste.
 
Back
Top