Welcome.Hello experts,
What would be the approach to recover Pd from graphite ore?
Pd is less than showed in the WD XRF.
ICP gives 760 ppm.
Ore composition attached.
Origin of ore is Afghanistan.Welcome.
What is the origin of the said Graphite ore?
How was the test done?
Origin of ore is Afghanistan.
Tests were done on ICP.
Origin of ore is Afghanistan.
Tests were done on ICP.
I was not referring to position, is it a proper ore or is it some product/byproduct from an industrial process?Origin of ore is Afghanistan.
Tests were done on ICP.
It's a proper run of mine ore.I was not referring to position, is it a proper ore or is it some product/byproduct from an industrial process?
How was the prill in the picture made?It's a proper run of mine ore.
The report also gives a hint.
What quality has the Graphite in the ore?It's a proper run of mine ore.
The report also gives a hint.
How was the prill in the picture made?
Cupelling?
How was the prill in the picture made?
Cupelling?