Crudmudgeon
Member
- Joined
- Aug 2, 2024
- Messages
- 8
I recently upsized my silver cell to a 5L stainless bowl. With 108g silver/L (1M) as silver nitrate, I am getting 10+A of current at 3V after 1hr of running. This seems unbelievably high... I don't recall seeing anyone report such amperage.
Is there any inherent problem for the silver at such high amps? Should I cut back to 2.5V to prevent copper codeposition and protect purity of the plated out crystals?
Thank you
Is there any inherent problem for the silver at such high amps? Should I cut back to 2.5V to prevent copper codeposition and protect purity of the plated out crystals?
Thank you