I was just processing some pins and contacts when I noticed how much of the fine gold power floated in the solution.
I first filtered the finished AP then collected it.
In the filters I found a blueish substance along with the gold foils and particles.
Rinse filter with hot water, part of the substances dissolves, passes trough filter and the rest turns orange.
Rinse filter with HCl and part of the substance disolves and passes trough filter. some grey substance remains, along with the goldparticles.
I still saw very small particle floating. So I decided to freeze the AP and then get the particles.
Put the filtered AP into plastic champagne glasses and let them freeze in a refrigerator.
A dark substance and fine gold powder was trappen in the bottom of the glass. Since it was narrow, it was easy to saw the dark end off and a blue fresh looking frozen AP remained as rest.
Repeated this with about 20 glasses and concentrated the settlements from the bottom of the glasses.
Added the expert from the filters since it looked the same.
After 3 times concentrating I had half a glass with grey substance mixed with gold powder and some larger foil on the bottom. Melted it.

Question now is: What do I have here? There is quite some gold powder that I colleted this way and there still is this grey substance which does not dissolve in HCl and seems to have a similiar density as gold since it always where the gold is.
Some of the grey stuff was able to pass the filter, some not.
How do I go on from here?
I first filtered the finished AP then collected it.
In the filters I found a blueish substance along with the gold foils and particles.
Rinse filter with hot water, part of the substances dissolves, passes trough filter and the rest turns orange.
Rinse filter with HCl and part of the substance disolves and passes trough filter. some grey substance remains, along with the goldparticles.
I still saw very small particle floating. So I decided to freeze the AP and then get the particles.
Put the filtered AP into plastic champagne glasses and let them freeze in a refrigerator.
A dark substance and fine gold powder was trappen in the bottom of the glass. Since it was narrow, it was easy to saw the dark end off and a blue fresh looking frozen AP remained as rest.
Repeated this with about 20 glasses and concentrated the settlements from the bottom of the glasses.
Added the expert from the filters since it looked the same.
After 3 times concentrating I had half a glass with grey substance mixed with gold powder and some larger foil on the bottom. Melted it.

Question now is: What do I have here? There is quite some gold powder that I colleted this way and there still is this grey substance which does not dissolve in HCl and seems to have a similiar density as gold since it always where the gold is.
Some of the grey stuff was able to pass the filter, some not.
How do I go on from here?