Hey all, how are things. I have recently received a batch of GF mesh watch bands and I was wondering if any one would care to share any tips or methods for these in particular. Bands of this type>>>
https://www.google.ca/searchq=gold+filled+mesh+watch+bands&hl=en&prmd=imvns&source=lnms&tbm=isch&ei=3kioT9HZJuqD6AHR7d2gBA&sa=X&oi=mode_link&ct=mode&cd=2&ved=0CC8Q_AUoAQ&biw=1024&bih=677
Other than a good incineration I am not sure if these should be done like other GF scrap. Generally I just break up GF and incinerate and dissolve in 50/50 nitric.
Thanks Mike.