If I'm understanding Bugbee correctly, I should not need to add any acidic flux, such as borax, because my ore is already mostly silica (quartz). Am I correct or misunderstanding something? If I were to concentrate the ore, then I might need to add borax/silica. If this it true, why use borax instead of just adding back some of the quartz that was panned out?
 
If I'm understanding Bugbee correctly, I should not need to add any acidic flux, such as borax, because my ore is already mostly silica (quartz). Am I correct or misunderstanding something? If I were to concentrate the ore, then I might need to add borax/silica. If this it true, why use borax instead of just adding back some of the quartz that was panned out?
The melting time will depend on crucible size, and amount of contents. Temp should be around 2000 F, maybe 50 degrees higher. Contents should be bone dry. Foaming is the release of CO2 evaporating off due to the heat reaction. Try using Sodium Hydroxide flakes for less boiling reaction. Litharge is far superior to metallic Lead for a collector. The amount of Silica needed, if any, will be determined by the erosion of the crucible. Not enough Silica, and it will eat the crucible, leading to spills. Some assay books will give the exact equation for concocting the correct flux. A knowledge of minerals and chemistry is required, otherwise you are at the approximation game of trial and error. Concentrates will change your recipe for the flux. If you go too heavy on the Soda Ash, it will eat the crucible. Read, then re read Bugbee some more. It takes a while for the chemistry of each flux, and the respective reactions, with each mineral in the sample.
 
I understand that you may have additional information and reasons to want to smelt this sample. But based on the information provided, there isn't enough value to pay for the flux. The sample is 34% Si and 6% minor elements. Most of the elements on the report were below detection limits. I would doubt that crushing, pulverizing and panning would significantly change the value.