hi. still very new at this. i try to read as much as possible on here before thinking of starting to recover gold.. i got a pretty good idea of the A/P process for pins but i was wondering what a good way to get the gold plate off the ram sticks and chips(green circuit boards as i call them). i don't want to try nitric acid or sulfiric because i don't know much of them and dont want to lose the gold i do have on the green boards.
so is there a easy way? like using the A/P process? i'm thinking now since there is not any basemetal in it but i'm just asking. and what about a cell using a battery charger and hcl or something?
i like the A/P process because i can see the gold i am getting...other processes i don't like because it disolves it and i gotta try to find it and get it back..
any help would be appreciated
 
duncan28 said:
and dont want to lose the gold
Just a quick note to commend you for using the correct word. You can't imagine the number of readers that use the word loose when they mean lose.

Well done!