Polski! 8)
Dave
Dave
4metals said:These are from a tunnelbar machine. They're nice too. Melted in nitrogen atmosphere in machined graphite.
image.jpeg
4metals said:These are from a tunnelbar machine. They're nice too. Melted in nitrogen atmosphere in machined graphite.
image.jpeg
Refining Rick said:My first poured bar. Think I need to get the graphite mold hotter.
Refining Rick said:My first poured bar. Think I need to get the graphite mold hotter.
anachronism said:Refining Rick said:My first poured bar. Think I need to get the graphite mold hotter.
That's not bad at all. Personally I'd heat the gold more before pouring it over- let it turn a bit brighter in the crucible if you're using a hot enough gas. Otherwise it's pretty good.