4metals said:
These are from a tunnelbar machine. They're nice too. Melted in nitrogen atmosphere in machined graphite.


image.jpeg

hi i know it's out of topic. can i ask how to make those? where i can find the step to make it or the machine?
in my country we just used traditional ways without safety or else
and the best i can get is just shinny top but not smooth on surface like that
people like that kind of gold because the appearance is good
 
Refining Rick said:
My first poured bar. Think I need to get the graphite mold hotter.

That's not bad at all. Personally I'd heat the gold more before pouring it over- let it turn a bit brighter in the crucible if you're using a hot enough gas. Otherwise it's pretty good.
 
anachronism said:
Refining Rick said:
My first poured bar. Think I need to get the graphite mold hotter.

That's not bad at all. Personally I'd heat the gold more before pouring it over- let it turn a bit brighter in the crucible if you're using a hot enough gas. Otherwise it's pretty good.

Keep the torch flame on it during the pour & make the pour just a bit off center of the mold

Its still a nice bar though 8)

Kurt
 
"just a little East coast color"

The color of gold :G is much preferable that the color of COLD a.k.a. SNOW!!