Hi .Where did this gold come from and how did you recover it?
Is it placer gold?
Do you have an assay or other tests that there is Gold in your "soil"?Hi .
I got this from yellow soil
I acidified first, then precipitated with ammonia. The sediment was white. Then I washed it with heat and the color turned brown. I am not really sure now, is this gold or iron? Can you help me? I guess it is gold because it is heavy. What is your solution in this matter, dear Mr. Martin?
If it is metallic gold concentrated by panning, you could test if some grains dissolve in AR in a test tube. Then test with stannous for pm's.Hi .
I got this from yellow soil
I acidified first, then precipitated with ammonia. The sediment was white. Then I washed it with heat and the color turned brown. I am not really sure now, is this gold or iron? Can you help me? I guess it is gold because it is heavy. What is your solution in this matter, dear Mr. Martin?
It is impossible to answer your question.Hello friends
When I directly acidified the soil, clouds formed on the surface of the soil that could not be dissolved in the acid solution. I separated them, dried them and washed them. This is his photo
I have moved the posts to your other acidified soil posts.Hello friends
When I directly acidified the soil, clouds formed on the surface of the soil that could not be dissolved in the acid solution. I separated them, dried them and washed them. This is his photo
Enter your email address to join: