Did a GF batch, nitric, rinse, nitric again, rinse, incinerate foils, HCL boil, followed by 3 distilled water boils. AR to dissolve gold.
Filtered to clear. Dropped with SMB, looked ok, then got this unusual white stuff in beaker?
Any thoughts? Think maybe tin or lead?
Going to do usual powder DW water and HCL rinse I think?
Thank you