Hi!

Some tests positive some negative. :)

One liter solution make by 18 grams mixed powders. Worth 0.57 dollar but only dissolve 0.6 grams of gold.
Zinc precipitation is best choice. Ph 6 and 4 grams of zinc per 1 gram Au.
Electrolysis works.
 
Hi!

This is a similar to eco goldex. No dangeros. After leach no need ammonia.Litle Naoh and cement zinc.

Content ferrocyanide. Prohibet acid adition.

At the proces no free cyanide.

Sorry i problems english. :)
Please we are interested in purchasing your reagent but at what PH Levels does it work? Because the vessels we use are limited to some pH levels
 
Please we are interested in purchasing your reagent but at what PH Levels does it work? Because the vessels we use are limited to some pH levels

FYI, unfortunately Elektrikis has not been here in a long time (last seen November 01, 2021). So it is unlikely your question will ever be answered.
 