ssharktu17
Well-known member
Hello guys, I have a couple ounces of scrap plated looking stuff with possibly some 14kt mixed in. So I am getting ready refine it. I have a mixture of sulfuric and nitric that is 30/30 will that work or will I end up with some additional precipitates? Its something used in cleaning stainless pipes from calcium deposits..