samuel-a
Well-known member
- Joined
- Oct 7, 2009
- Messages
- 2,190
I've been wanting to try this idea for a while now...
With a dremmel tool i "carved" these trenches in the plastic funnel.
With a turbid solution (Ar+AgCl), the speed improved from about one drop every 1 - 1.5 seconds to 1.5 - 2 drops per second, that's almost twice as fast...
I guess the dipper they are, the higher the speed could be...
Though i usually use vacuum, occasionally, i do find myself needing to use gravity filtration.
Edit: spelling
With a dremmel tool i "carved" these trenches in the plastic funnel.
With a turbid solution (Ar+AgCl), the speed improved from about one drop every 1 - 1.5 seconds to 1.5 - 2 drops per second, that's almost twice as fast...
I guess the dipper they are, the higher the speed could be...
Though i usually use vacuum, occasionally, i do find myself needing to use gravity filtration.
Edit: spelling