I have some green copper nitrate. At least I think it's copper nitrate. It's silver dissolved in nitric acid, but the resulting solution is green and not blue like I expected. I added copper bars and they immediately started cementing (I assume silver) almost instantly. I tried to post a picture but couldn't. Any thoughts or comments? Or suggestions? Thanks,