Hello everyone. I came accross some cheap scrap computer waste for refining. I know the content is low. But figure if I would start with 3 kilos. I need 3 grams of gold to break even. I figure the gold content is more then .1%. And I am ok if I lose money. My curiosity got to me and had to give it a shot. At least will learn something.To refine and see what I get out of it. But wondering if anyone has an idea what to expect. If I take it to a gold buyer for scanning can they determine the content. How does the scanning work. And what should I expect for refining cost. I am in Barrie Ontario. There is a place in Orilla but I didn't like there way of doing things. There is another in Brampton that I think I will use. But still waiting to hear back. Any advice would be appreciated.
 
Hello everyone. I came accross some cheap scrap computer waste for refining. I know the content is low. But figure if I would start with 3 kilos. I need 3 grams of gold to break even. I figure the gold content is more then .1%. And I am ok if I lose money. My curiosity got to me and had to give it a shot. At least will learn something.To refine and see what I get out of it. But wondering if anyone has an idea what to expect. If I take it to a gold buyer for scanning can they determine the content. How does the scanning work. And what should I expect for refining cost. I am in Barrie Ontario. There is a place in Orilla but I didn't like there way of doing things. There is another in Brampton that I think I will use. But still waiting to hear back. Any advice would be appreciated.
Welcome to us.

Sorry to be the bearer of bad news.
What can you expect?
Well if it is an Ebay, Alibaba or other online source you can expect nothing.
If you are lucky there is enough to see a few dusty grains in the bottom of the beaker.
1 gram per kilo is highly unlikely, if you get even a tenth of a gram consider yourself lucky.
So if you have not received it yet, cancel the order, the best scammers gild the brass, the rest don't even bother with that.

In the mean time read these links:

We ask our new members to do 3 things.
1. Read C.M. Hokes book on refining jewelers scrap, it gives an easy introduction to the most important chemistry regarding refining.
It is free here on the forum: https://goldrefiningforum.com/phpBB3/viewtopic.php?f=54&t=19798
2. Then read the safety section of the forum: https://goldrefiningforum.com/forums/safety.47/
3. And then read about "Dealing with waste" in the forum: https://goldrefiningforum.com/threads/dealing-with-waste.10539/

Suggested reading:
https://goldrefiningforum.com/forums/the-library.101/
https://goldrefiningforum.com/threads/when-in-doubt-cement-it-out.30236/
https://goldrefiningforum.com/threa...le-read-this-before-you-post-about-ore.33333/


Forum rules is here.
https://goldrefiningforum.com/threads/gold-refining-forum-rules.31182/
 
Hi Jory, Welcome.

You got 6.6 pounds of what type of computer scrap?
And you need 3 grams to break even.
Your title states melted computer components.
As Ygg states: Sorry to be the bearer of bad news.
If these are those melted bars of computer scrap, get a refund or make a door weight holder or put them on the shelf and don't waste any more time on them.
 

Attachments

  • 20241025_101029.jpg
    20241025_101029.jpg
    970.2 KB
Thanks. For the info. I had it scanned. It is very low content but the said there is about 1 karat a bit under. 1 karat is 4.1% gold content if I am correct. So I figure it has to be 1% content for sure. But I don't know much about refining cost. The couple places I called what to refine it and give me cash after. I want to pay for the refining and keep whatever it yields. I have some jewelry to mix in.
 
Thanks. For the info. I had it scanned. It is very low content but the said there is about 1 karat a bit under. 1 karat is 4.1% gold content if I am correct. So I figure it has to be 1% content for sure. But I don't know much about refining cost. The couple places I called what to refine it and give me cash after. I want to pay for the refining and keep whatever it yields. I have some jewelry to mix in.
Keep the jewelry apart, I suspect the guy who tested it failed to inform about thresholds and even was a bit kind to not let you down too much.
Known jewelry is totally different ballgame.
 
If it's mainly comprised of copper, use in your stock pot. IF, there is any PM's in it you'll eventually recover it.

That way you can save all your clean copper for the scrapyard and get paid top dollar for it.
Doing g some research I like the qupeal method. Could see making small buttons, and then melt the buttons and pour a bigger piece.
 
Doing g some research I like the qupeal method. Could see making small buttons, and then melt the buttons and pour a bigger piece.
Too high Copper content is not ideal for cupeling.
Cupels are most of the time used for fire assays and similar testing to assess the amount of PMs in ore and such bodies.
I is really not very good for production even though it can be done.
You will need an electric furnace with front opening so you can have good temperature control and access to oxygen.
 
Trying to learn more how to refine with borax. Hard to find a good video.
Borax is not used for refining.
It is more a protective flux.
Smelting will refine/concentrate to a certain degree but is not considered actual refining.
The science behind proper fluxing is a study by itself.

Have you read and studied the links you were given?
 