hcl+clorox. got to smb and it wont drop.

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

chris.bozman42

Well-known member
Joined
May 1, 2011
Messages
47
ok i have dissolved some sulphuric cell black sludge and some gold leaf in muriatic and clorox. everything went beautiful. for some reason the color is green. i know there was a minuscule amount of copper dust. and i mean one millionth of a grams worth. filtered and added some water. distilled...when washing filter. now the solution is crystal clear green. smb has been added and nothing is happening. if you can lead me in the right direction it will be greatly appreciated.
 
ok nevermind! it is dropping now! just threw it on the hot plate and 5 mins later its dropping like a champ!
 