paulo123
New member
Hi there. I have almost 500 grams of gold fingers , I have taken the gold
flakes from the plastics and cut of the wires with a opperation knive-side cutter , so these 500 grams have no plastics-fiber and they only need to be put to the acids and I need to know :
How much hydrogen peroxide and muriatic acid is needed for a batch of 100 grams of gold flakes.
paulo123
flakes from the plastics and cut of the wires with a opperation knive-side cutter , so these 500 grams have no plastics-fiber and they only need to be put to the acids and I need to know :
How much hydrogen peroxide and muriatic acid is needed for a batch of 100 grams of gold flakes.
paulo123