razvanflorin said:
if someone has any suggestion on smelting the gold foils please leave a comment below ! :idea: :mrgreen:
Razvan, you are not smelting your foils. You are simply melting them.
When you heat a metal until it changes from a solid to a liquid, you are melting, just like heating an ice cube till it melts.
Smelting also uses heat, and any metals become liquid, but it also involves fluxes that cause the material to undergo chemical changes. Smelting may be used to process ore concentrates, circuit boards, MLCCs, etc.
Dave