Welcome to us.View attachment 65224 can somebody please tell me what I have in solution? This is a status chloride test That I used on a catalytic converter. Substrate chlorine leach solution!
View attachment 65224 can somebody please tell me what I have in solution? This is a status chloride test That I used on a catalytic converter. Substrate chlorine leach solution!
This means:Set things aside
So I have a question, since I never made it to the point of actually dropping the salts from the solution. I only made it to the point of leaching I never went a step after that, is the solution still dangerous at the point of leaching as well or is it only when the Platinum salts are dropped? I'll be my fucking?Mucking around with PGMs without a proven plan. Got it. If you do not follow the advice of Martijn, you will kill yourself. Or worse, you may destroy enough function of your lungs, kidneys, or liver to the point of abject misery and debilitation for several years before your body does die.
Should you actually get yourself tested for exposure to the toxic salts you have created, be completely honest with ALL the medical professionals connected with your case.
Have fun.
Time for more coffee.
You dissolved the metals, then they become salts.So I have a question, since I never made it to the point of actually dropping the salts from the solution. I only made it to the point of leaching I never went a step after that, is the solution still dangerous at the point of leaching as well or is it only when the Platinum salts are dropped? I'll be my fucking?
Oh my God, I literally had it on my skin multiple times and almost died when I accidentally inhaled the chlorine gas! What's going to happen to me?You dissolved the metals, then they become salts.
As dissolved salts it is in the most dangerous form.
Go to the doctor and tell him everything.Oh my God, I literally had it on my skin multiple times and almost died when I accidentally inhaled the chlorine gas! What's going to happen to me?