If your melt dish is glazed with Borax there is just hitting it with enough heat and time to let it pool together.Very happy to announce my first relatively successful recovery and melt 😃 haven't quite mastered the melt dish removal yet.
Thanks for your patience and advice... 😉
In fairness that looks pretty good!Very happy to announce my first relatively successful recovery and melt 😃 haven't quite mastered the melt dish removal yet.
Thanks for your patience and advice... 😉
Very happy to announce my first relatively successful recovery and melt 😃 haven't quite mastered the melt dish removal yet.
Thanks for your patience and advice... 😉
ThanksIt looks great to me!
Dave
No I don't, I will next time, tksDo you use insulation around your melting dish.
Thanks...Agreed looks pretty decent , when it comes to removal from the melt dish once it’s pooled together remove your flame and wait for the bead to flash over give a few seconds and remove with tweezers or pliers and drop into cold water.
Cheers...In fairness that looks pretty good!