All,

I built a bowl trying to mimic what Sam had done here, I ran the left over ash from panning, here are result, the bowl is cake funnel.

The BB,
View attachment 25760

My blue well gray bowl in action,
View attachment 25761

Almost finished cleaning the junk from the heavy metals,
View attachment 25762

I learned the angel and location of the water hose is very critical also water pressure, so valve is a must in this system, plus eventhough I had used mortat pestel to grind the ash, and filter, still I could see poder size along bigger sizes mixed, so a homogenius sizing will improve the performance and control the loss.
Addition of liquid soap is a must.

Will try more experiments tommorow.

Regards
Krvin
for rough seperation, this will work but for fines, i belive the vortex smoothness
created by a tube in the funnel makes the best cleaner (that the blue bowl can give) ..
 
Last edited:
Good work Sam
Here are 2 pics of my Blue Bowl so you can see where they bring in the water and the slope of the cone to help fine tune what goes out the top.
Maybe use a tall funnel and cut the spout off to get the sloped cone, it might work.

PS. pardon the dust. I haven't used it yet this year.