I am getting ready to mix up my SMB and try dropping my Gold, Problem is my shops Tempature is 40-50 Degrees with the chemicals about the same, Will this have any effect?
joehast said:My experience has been harder to drop my auric chloride when temps are so low in my work area. I have solved this by slowly heating diluted HCL/CL with a heat plate(not very hot,just warm). However, I still have a problem w/ultra fine gold particles floating to top of the rinse water, and then poured out down the drain.