What do I scoop that gold slopes out with? Can't use a spoon.
 

Attachments

  • Screenshot_20250219_165243_Snapchat.jpg
    Screenshot_20250219_165243_Snapchat.jpg
    1.3 MB
  • Screenshot_20250219_165253_Snapchat.jpg
    Screenshot_20250219_165253_Snapchat.jpg
    1.7 MB
Holy crap is that the drop?
That'd be the biggest drop I've ever seen
All the slop is in the other dish fermenting more aqua regia
 

Attachments

  • Screenshot_20250219_190101_Snapchat.jpg
    Screenshot_20250219_190101_Snapchat.jpg
    1 MB
  • Screenshot_20250219_190054_Snapchat.jpg
    Screenshot_20250219_190054_Snapchat.jpg
    915.6 KB
Might make a sluice out of furnace filter.
Gonna straw filter tomorrow. And I've got a ton of gold stuck in the crucible I just started trying to overheat for pouring. I can test dissolving it in hot water before I consider adding it to the solution.
 
Might make a sluice out of furnace filter.
Gonna straw filter tomorrow. And I've got a ton of gold stuck in the crucible I just started trying to overheat for pouring. I can test dissolving it in hot water before I consider adding it to the solution.
You really need to stop and start to study.
You are not making sense at all.
Our patience are streched quite far already.
 
This looks nothing like Gold.
It looks like sand and Iron salts.
Aqua Regia do not ferment.
It is made by mixing Nitric and HCl.
So how did you drop it?
The Iron Sulfide causes it to drop. It turns the reaction green like glass when it finally forces all of the AU to precipitate. Time pressure reaction all can cause the drop, in this case the small amount of Iron contamination. I got pretty lucky there.

It's pure gold drop with slight silver puddy content. I got that entire pyrex dried out now chalk full of mostly silver puddy and borax puddy.

In response to the moderator, a Fren showed me this straw funnel method, pic related. And apparently borax slag dissolves in boiling water., which is a big deal. Should've dissolved it and Extracted before I used acid.
 

Attachments

  • Screenshot_20250219_192319_Snapchat.jpg
    Screenshot_20250219_192319_Snapchat.jpg
    1.4 MB
  • Screenshot_20250219_223417_Snapchat.jpg
    Screenshot_20250219_223417_Snapchat.jpg
    1.6 MB
The Iron Sulfide causes it to drop. It turns the reaction green like glass when it finally forces all of the AU to precipitate. Time pressure reaction all can cause the drop, in this case the small amount of Iron contamination. I got pretty lucky there.

It's pure gold drop with slight silver puddy content. I got that entire pyrex dried out now chalk full of mostly silver puddy and borax puddy.

In response to the moderator, a Fren showed me this straw funnel method, pic related. And apparently borax slag dissolves in boiling water., which is a big deal. Should've dissolved it and Extracted before I used acid.
 

Attachments

  • Screenshot_20250220_094324_Messenger.jpg
    Screenshot_20250220_094324_Messenger.jpg
    1 MB
The Iron Sulfide causes it to drop. It turns the reaction green like glass when it finally forces all of the AU to precipitate. Time pressure reaction all can cause the drop, in this case the small amount of Iron contamination. I got pretty lucky there.

It's pure gold drop with slight silver puddy content. I got that entire pyrex dried out now chalk full of mostly silver puddy and borax puddy.

In response to the moderator, a Fren showed me this straw funnel method, pic related. And apparently borax slag dissolves in boiling water., which is a big deal. Should've dissolved it and Extracted before I used acid.
Sulfides do not drop Gold, Sulfites do and one Sulfate I know of, namel Iron Sulfate.
Sulfides, Sulfites and Sulfates are totally different animals i chemistry.
How is your studies going?
 