Ran some gold trimmed/painted cups and such through HCL/CL last night along with a little powder from a previous mess up. Abought the size of a match heads worth. Here are some photos.
*sand is on the outside of the glass*
*definite positive for gold*
Will drop with some metabisulfite tonight and see what was recovered.
Happy Hunting!
![1001897j.jpg](https://proxy.imagearchive.com/c50/c500429e4e7109c5dfb62ce97ae3e446.jpg)
*sand is on the outside of the glass*
![1001901y.jpg](https://proxy.imagearchive.com/909/909b393ab8623598ea4cdffa443f2cbb.jpg)
*definite positive for gold*
Will drop with some metabisulfite tonight and see what was recovered.
Happy Hunting!