Can someone help me smelt/refine a gold concentrate derived from crushed rock that was then panned. I have purchased a small propane kiln w/ large crusable,made of dark agroget material, that I've been told I need to seal first,and I have borax at the ready and about 15 to 20 Oz of concitrate,would prefer to start out with batches of 5 oz's of concintrate,thanks,tod Williams, e-mail:****[email protected] or cell phone:***-440-3319
Welcome.
I'm not sure leaving your email and phone number in the open like this is a good move.
 
Last edited:
Can someone help me smelt/refine a gold concentrate derived from crushed rock that was then panned. I have purchased a small propane kiln w/ large crusable,made of dark agroget material, that I've been told I need to seal first,and I have borax at the ready and about 15 to 20 Oz of concitrate,would prefer to start out with batches of 5 oz's of concintrate,thanks,tod Williams, e-mail:***[email protected] or cell phone:***-440-3319

Edit by moderator to hide real mail and telephone.
Better use the Conversation/PM mode to contact someone.

Per the bold print in the above quote - it doesn't do much good to edit the phone number & email in this OP when it is still available in the quote in the very next post posted by Yggdrasil

Kurt
 
In Northeast Ohio, the brick and mortor shops offer 93-97.5% of spot. Are there any Reputable/Trustworthy sites you could send it to in order to get closer to spot? Seems like a year ago everyone was offering 98% of spot.
 