Hey everyone, it's been a while...circumstances have made it impossible for me to do any kind of refining. But I am looking for some help. I'm in Newmarket, Ontario, Canada, I purchased three 2025 $5 Canadian Maple Leafs, that I suspect are fake. Because I used paypal to buy them I was able to get my money back, it was one of those too good to be true type things. Anyway, I have a pocket pinger, (all of my test solutions have gone bad) I have never been able to get a reliable ping test even with a legit coin. Anyway for some odd reason, holding one in my hand, it tells me something is off with them. I've pinged them (again never been good with that), I've weighed them (seems good), and measured them (spot on). Thing is I accidently dropped one on the floor and I expected to hear something but didn't. Anyway, I'm looking for someone near me who could reliably test them to see if my thoughts are confirmed. I'd rather have someone come by to test them but I know that is unrealistic. I can mail them to whomever, if they are good we can go from there, if they are fake as I suspect, they can be dealt with. Anyway let me know I'll be watching my email.

Thanks,

Rusty
 
Rusty, if you have an accurate scale, you can check the specific gravity. For small coins, you'll want something that can weigh accurate to .01 grams.

If you have a scale, I can explain the test. It's pretty simple.

Dave
 
Weigh the coin.

Next, tie a thin thread or string around the coin.

Fill a small beaker or container with water. Put it on the scale and tare it or record the weight.

Hold the thread and lower the coin into the water till it is submerged. Don't allow it to touch the container. Record the weight of the water that has been displaced.

Divide the dry weight of the coin by the weight of the water that has been displaced. The result is the specific gravity.

Dave
 
A procedure to measure specific gravity:
1: weigh the coin dry, write down weight 1 in grams
2: weigh the coin in water hanging from a very thin wire, completely submerged, but not touching the bottom. Do this by taring the scale with the water beaker before you weigh it with the coin. write down weight 2.
Divide weight 1 by weight 2
The number you get is the specific gravity aka density in grams/ml
or kg/liter.
Both tungsten and gold have a 19.3 specific gravity.
 
A procedure to measure specific gravity:
1: weigh the coin dry, write down weight 1 in grams
2: weigh the coin in water hanging from a very thin wire, completely submerged, but not touching the bottom. Do this by taring the scale with the water beaker before you weigh it with the coin. write down weight 2.
Divide weight 1 by weight 2
The number you get is the specific gravity aka density in grams/ml
or kg/liter.
Both tungsten and gold have a 19.3 specific gravity.
What's the specific gravity of 1oz 9999 Silver Maple Leaf?
 