I thought I would post these. I found them some time ago, but didn't think to post them until I read this post.

If this is not appropriate please let me know, I don't want to step on another person's hard work, and it seems Geo has put a lot of thought into this.

EDITED -- Keep in mind that all these processes should only be attempted if you are skilled and knowledgeable enough to do them safely. Some of the posted video's may not show the best ways to be safe. If there is any question as to how to do anything safely, you should ask or check with someone who knows before you attempt anything -- EDITED

The "NurdRage" YouTube channel has a lot of useful video's on many of the things we use in recovering and refining. Here are videos on making acids.

Nitric Acid
[youtube]http://www.youtube.com/watch?v=2yE7v4wkuZU[/youtube]

Sulfuric Acid
[youtube]http://www.youtube.com/watch?v=okvvD3-DF9U&feature=channel&list=UL[/youtube]

Hydrochloric Acid
[youtube]http://www.youtube.com/watch?v=YGjd7xxTuZw&feature=relmfu[/youtube]

Also a video on Stump Remover
[youtube]http://www.youtube.com/watch?v=IG-fvPHzEoc&feature=channel&list=UL[/youtube]

More in the next post
 
Also thee YouTube channel Science Hideout has a lot of good chemistry videos, some for making acid also:

TWO Nitric Acid methods
[youtube]http://www.youtube.com/watch?v=NMrWz06RtD4&feature=related[/youtube]

[youtube]http://www.youtube.com/watch?v=vGDMWgbzlrs&feature=channel&list=UL[/youtube]

Good video on Hydrochloric Acid
[youtube]http://www.youtube.com/watch?v=ugdJfTewQ_8&feature=channel&list=UL[/youtube]

Glacial Acetic Acid
[youtube]http://www.youtube.com/watch?v=04GInkGHGFM&feature=channel&list=UL[/youtube]
 
Here is a very different way to make Nitric Acid without a Nitrate Salt!

[youtube]http://www.youtube.com/watch?v=xYrl8mPg8Ag&feature=related[/youtube]

Yet another method of making Nitric Acid
[youtube]http://www.youtube.com/watch?v=TtPiwbRA4N8[/youtube]

One more video on making Nitric Acid
[youtube]http://www.youtube.com/watch?v=1_VY9rB4U1E[/youtube]

There are literally a ton of video's that are excellent to watch, about Chemistry that pertain to what we do.

Scott
 
yep, theres alot of good videos on youtube. theres also alot of videos that not only convey misinformation, they can be downright dangerous.any and all information from youtube or anywhere else on the internet should be double checked here for accuracy before trying any experiment found there.
 