• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Chemical Need 10% Nitric Acid to 68%

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

talalstuvs

Well-known member
Joined
Sep 5, 2010
Messages
52
I have 68 % nitirc i want 10% of Nitric Acid what would be it's ration and calculation to add water? waiting for urs reply.
 
I belive you can use the density tabel from link below :

You olso have a calculator on top of the page.

http://www.handymath.com/cgi-bin/nitrictble2.cgi?submit=Entry
 
One of those simple, but confusing, math problems. An involved equation could surely be derived for this but, instead, here is a fairly straightforward logical method (assuming I didn't get confused).

According to the chart in the link above, using a temp of 20C:
1 ml of 68% HNO3 weighs 1.4048 grams
1 ml of 10% HNO3 weighs 1.0543 grams

Therefore:
1 liter of 68% weighs 1404.8 g
1 liter of 10% weighs 1054.3 g

Therefore:
1 liter of 68% contains 1404.8 x .68 = 955.3 g of HNO3
1 liter of 10% contains 1054.3 x .10 = 105.4 g of HNO3

Therefore:
To make up 1 liter of 10%, it will take (105.4/955.3) x 1000 = 110 ml of 68% HNO3 + 890 ml of distilled water.
 
goldsilverpro said:
One of those simple, but confusing, math problems. An involved equation could surely be derived for this but, instead, here is a fairly straightforward logical method (assuming I didn't get confused).

According to the chart in the link above, using a temp of 20C:
1 ml of 68% HNO3 weighs 1.4048 grams
1 ml of 10% HNO3 weighs 1.0543 grams

Therefore:
1 liter of 68% weighs 1404.8 g
1 liter of 10% weighs 1054.3 g

Therefore:
1 liter of 68% contains 1404.8 x .68 = 955.3 g of HNO3
1 liter of 10% contains 1054.3 x .10 = 105.4 g of HNO3

Therefore:
To make up 1 liter of 10%, it will take (105.4/955.3) x 1000 = 110 ml of 68% HNO3 + 890 ml of distilled water.

They put questions like this all over the GMATS - I hated them.
 
I want to determine the concentration of my HNO3 - so I went looking for the info here at GRF & on the WWW.

Because web sites do go off-line and the information is very useful, I am re-posting some of it here. If that is bad form/ etiquette in this instance please let me know.

Also, starting at 64% in the left-most column (HNO3/nitric acid concentration), that 1.4078 belongs in the 5 degree C column - the formatting gets slightly garbled in translation.

In the 65% column, 1.4128 is in the 5% column. In the 100% column, 1.5402 is in the 5% column. etc.

Key-words ~ Nitric Acid Concentration, Density, Specific Gravity -

Nitric Acid Solutions in Water
Temperature in degrees Centigrade (°C)
0°C 5°C 10°C 15°C 20°C 25°C 30°C 40°C 50°C 60°C 80°C 100°C
Concentration (% Weight) Density (kg/L)
1 1.0058 1.00572 1.00534 1.00464 1.00364 1.00241 1.0009 0.9973 0.9931 0.9882 0.9767 0.9632
2 1.0117 1.01149 1.01099 1.01018 1.00909 1.00778 1.0061 1.0025 0.9982 0.9932 0.9816 0.9681
3 1.0176 1.0173 1.01668 1.01576 1.01457 1.01318 1.0114 1.0077 1.0033 0.9982 0.9865 0.973
4 1.0236 1.02315 1.0224 1.02137 1.02008 1.01861 1.0168 1.0129 1.0084 1.0033 0.9915 0.9779
5 1.0296 1.02904 1.02816 1.02702 1.02563 1.02408 1.0222 1.0182 1.0136 1.0084 0.9965 0.9829
6 1.0357 1.03497 1.03397 1.03272 1.03122 1.02958 1.0277 1.0235 1.0188 1.0136 1.0015 0.9879
7 1.0418 1.041 1.0399 1.0385 1.0369 1.0352 1.0333 1.0289 1.0241 1.0188 1.0066 0.9929
8 1.048 1.0471 1.0458 1.0443 1.0427 1.0409 1.0389 1.0344 1.0295 1.0241 1.0117 0.998
9 1.0543 1.0532 1.0518 1.0502 1.0485 1.0466 1.0446 1.0399 1.0349 1.0294 1.0169 1.0032
10 1.0606 1.0594 1.0578 1.0561 1.0543 1.0523 1.0503 1.0455 1.0403 1.0347 1.0221 1.0083
11 1.0669 1.0656 1.0639 1.0621 1.0602 1.0581 1.056 1.0511 1.0458 1.0401 1.0273 1.0134
12 1.0733 1.0718 1.07 1.0681 1.0661 1.064 1.0618 1.0567 1.0513 1.0455 1.0326 1.0186
13 1.0797 1.0781 1.0762 1.0742 1.0721 1.0699 1.0676 1.0624 1.0568 1.0509 1.0379 1.0238
14 1.0862 1.0845 1.0824 1.0803 1.0781 1.0758 1.0735 1.0681 1.0624 1.0564 1.0432 1.0289
15 1.0927 1.0909 1.0887 1.0865 1.0842 1.0818 1.0794 1.0739 1.068 1.0619 1.0485 1.0341
16 1.0992 1.0973 1.095 1.0927 1.0903 1.0879 1.0854 1.0797 1.0737 1.0675 1.0538 1.0393
17 1.1057 1.1038 1.1014 1.0989 1.0964 1.094 1.0914 1.0855 1.0794 1.0731 1.0592 1.0444
18 1.1123 1.1103 1.1078 1.1052 1.1026 1.1001 1.0974 1.0913 1.0851 1.0787 1.0646 1.0496
19 1.1189 1.1168 1.1142 1.1115 1.1088 1.1062 1.1034 1.0972 1.0908 1.0843 1.07 1.0547
20 1.1255 1.1234 1.1206 1.1178 1.115 1.1123 1.1094 1.1031 1.0966 1.0899 1.0754 1.0598
21 1.1322 1.13 1.1271 1.1242 1.1213 1.1185 1.1155 1.109 1.1024 1.0956 1.0808 1.065
22 1.1389 1.1366 1.1336 1.1306 1.1276 1.1247 1.1217 1.115 1.1083 1.1013 1.0862 1.0701
23 1.1457 1.1433 1.1402 1.1371 1.134 1.131 1.128 1.121 1.1142 1.107 1.0917 1.0753
24 1.1525 1.1501 1.1469 1.1437 1.1404 1.1374 1.1343 1.1271 1.1201 1.1127 1.0972 1.0805
25 1.1594 1.1569 1.1536 1.1503 1.1469 1.1438 1.1406 1.1332 1.126 1.1185 1.1027 1.0857
26 1.1663 1.1638 1.1603 1.1569 1.1534 1.1502 1.1469 1.1394 1.132 1.1244 1.1083 1.091
27 1.1733 1.1707 1.167 1.1635 1.16 1.1566 1.1533 1.1456 1.1381 1.1303 1.1139 1.0963
28 1.1803 1.1777 1.1738 1.1702 1.1666 1.1631 1.1597 1.1519 1.1442 1.1362 1.1195 1.1016
29 1.1874 1.1847 1.1807 1.177 1.1733 1.1697 1.1662 1.1582 1.1503 1.1422 1.1251 1.1069
30 1.1945 1.1917 1.1876 1.1838 1.18 1.1763 1.1727 1.1645 1.1564 1.1482 1.1307 1.1122
31 1.2016 1.1988 1.1945 1.1906 1.1867 1.1829 1.1792 1.1708 1.1625 1.1542 1.1363 1.1175
32 1.2088 1.2059 1.2014 1.1974 1.1934 1.1896 1.1857 1.1772 1.1687 1.1602 1.1419 1.1228
33 1.216 1.2131 1.2084 1.2043 1.2002 1.1963 1.1922 1.1836 1.1749 1.1662 1.1476 1.1281
34 1.2233 1.2203 1.2155 1.2113 1.2071 1.203 1.1988 1.1901 1.1812 1.1723 1.1533 1.1335
35 1.2306 1.2275 1.2227 1.2183 1.214 1.2098 1.2055 1.1966 1.1876 1.1784 1.1591 1.139
36 1.2375 1.2344 1.294 1.2249 1.2205 1.2163 1.2119 1.2028 1.1936 1.1842 1.1645 1.144
37 1.2444 1.2412 1.2361 1.2315 1.227 1.2227 1.2182 1.2089 1.1995 1.1899 1.1699 1.149
38 1.2513 1.2479 1.2428 1.2381 1.2335 1.2291 1.2245 1.215 1.2054 1.1956 1.1752 1.154
39 1.2581 1.2546 1.2494 1.2446 1.2399 1.2354 1.2308 1.221 1.2112 1.2013 1.1805 1.1589
40 1.2649 1.2613 1.256 1.2511 1.2463 1.2417 1.237 1.227 1.217 1.2069 1.1858 1.1638
41 1.2717 1.268 1.2626 1.2576 1.2527 1.248 1.2432 1.233 1.2229 1.2126 1.1911 1.1687
42 1.2786 1.2747 1.2692 1.2641 1.2591 1.2543 1.2494 1.239 1.2287 1.2182 1.1963 1.1735
43 1.2854 1.2814 1.2758 1.2706 1.2655 1.2606 1.2556 1.245 1.2345 1.2238 1.2015 1.1783
44 1.2922 1.288 1.2824 1.2771 1.2719 1.2669 1.2618 1.251 1.2403 1.2294 1.2067 1.1831
45 1.299 1.2947 1.289 1.2836 1.2783 1.2732 1.268 1.257 1.2461 1.235 1.2119 1.1879
46 1.3058 1.3014 1.2955 1.2901 1.2847 1.2795 1.2742 1.263 1.2519 1.2406 1.2171 1.1927
47 1.3126 1.308 1.3021 1.2966 1.2911 1.2858 1.2804 1.269 1.2577 1.2462 1.2223 1.1976
48 1.3194 1.3147 1.3087 1.3031 1.2975 1.2921 1.2867 1.275 1.2635 1.2518 1.2275 1.2024
49 1.3263 1.3214 1.3153 1.3096 1.304 1.2984 1.2929 1.2811 1.2693 1.2575 1.2328 1.2073
50 1.3327 1.3277 1.3215 1.3157 1.31 1.3043 1.2987 1.2867 1.2748 1.2628 1.2377 1.2118
51 1.3391 1.3339 1.3277 1.3218 1.316 1.3102 1.3045 1.2923 1.2802 1.268 1.2425 1.2163
52 1.3454 1.3401 1.3338 1.3278 1.3219 1.316 1.3102 1.2978 1.2856 1.2731 1.2473 1.2208
53 1.3517 1.3462 1.3399 1.3338 1.3278 1.3218 1.3159 1.3033 1.2909 1.2782 1.2521 1.2252
54 1.3579 1.3523 1.3459 1.3397 1.3336 1.3275 1.3215 1.3087 1.2961 1.2833 1.2568 1.2296
55 1.364 1.3583 1.3518 1.3455 1.3393 1.3331 1.327 1.3141 1.3013 1.2883 1.2615 1.2339
56 1.37 1.3642 1.3576 1.3512 1.3449 1.3386 1.3324 1.3194 1.3064 1.2932 1.2661 1.2382
57 1.3759 1.37 1.3634 1.3569 1.3505 1.3441 1.3377 1.3246 1.3114 1.2981 1.2706 1.2424
58 1.3818 1.3757 1.3691 1.3625 1.356 1.3495 1.343 1.3298 1.3164 1.3029 1.2751 1.2466
59 1.3875 1.3813 1.3747 1.368 1.3614 1.3548 1.3482 1.3348 1.3213 1.3077 1.2795 1.2507
60 1.3931 1.3868 1.3801 1.3734 1.3667 1.36 1.3533 1.3398 1.3261 1.3124 1.2839 1.2547
61 1.3986 1.3922 1.3855 1.3787 1.3719 1.3651 1.3583 1.3447 1.3308 1.3169 1.2881 1.2587
62 1.4039 1.3975 1.3907 1.3838 1.3769 1.37 1.3632 1.3494 1.3354 1.3213 1.2922 1.2625
63 1.4091 1.4027 1.3958 1.3888 1.3818 1.3748 1.3679 1.354 1.3398 1.3255 1.2962 1.2661
64 1.4078 1.4007 1.3936 1.3866 1.3795 1.3725
65 1.4128 1.4055 1.3984 1.3913 1.3841 1.377
66 1.4177 1.4103 1.4031 1.3959 1.3887 1.3814
67 1.4224 1.415 1.4077 1.4004 1.3932 1.3857
68 1.4271 1.4196 1.4122 1.4048 1.3976 1.39
69 1.4317 1.4241 1.4166 1.4091 1.4019 1.3942
70 1.4362 1.4285 1.421 1.4134 1.4061 1.3983
71 1.4406 1.4328 1.4252 1.4176 1.4102 1.4023
72 1.4449 1.4371 1.4294 1.4218 1.4142 1.4063
73 1.4491 1.4413 1.4335 1.4258 1.4182 1.4103
74 1.4532 1.4454 1.4376 1.4298 1.4221 1.4142
75 1.4573 1.4494 1.4415 1.4337 1.4259 1.418
76 1.4613 1.4533 1.4454 1.4375 1.4296 1.4217
77 1.4652 1.4572 1.4492 1.4413 1.4333 1.4253
78 1.469 1.461 1.4529 1.445 1.4369 1.4288
79 1.4727 1.4647 1.4565 1.4486 1.4404 1.4323
80 1.4764 1.4683 1.4601 1.4521 1.4439 1.4357
81 1.48 1.4718 1.4636 1.4555 1.4473 1.4391
82 1.4835 1.4753 1.467 1.4589 1.4507 1.4424
83 1.4869 1.4787 1.4704 1.4622 1.454 1.4456
84 1.4903 1.482 1.4737 1.4655 1.4572 1.4487
85 1.4936 1.4852 1.4769 1.4686 1.4603 1.4518
86 1.4968 1.4883 1.4799 1.4716 1.4633 1.4548
87 1.4999 1.4913 1.4829 1.4745 1.4662 1.4577
88 1.5029 1.4942 1.4858 1.4773 1.469 1.4605
89 1.5058 1.497 1.4885 1.48 1.4716 1.4631
90 1.5085 1.4997 1.4911 1.4826 1.4741 1.4656
91 1.5111 1.5023 1.4936 1.485 1.4766 1.4681
92 1.5136 1.5048 1.496 1.4873 1.4789 1.4704
93 1.5156 1.5068 1.4979 1.4892 1.4807 1.4722
94 1.5177 1.5088 1.4999 1.4912 1.4826 1.4741
95 1.5198 1.5109 1.5019 1.4932 1.4846 1.4761
96 1.522 1.513 1.504 1.4952 1.4867 1.4781
97 1.5244 1.5152 1.5062 1.4974 1.4889 1.4802
98 1.5278 1.5187 1.5096 1.5008 1.4922 1.4835
99 1.5327 1.5235 1.5144 1.5056 1.4969 1.4881
100 1.5402 1.531 1.5217 1.5129 1.504 1.4952
 

Latest posts

Back
Top