Acetic acid 5% and 3% h2o2 doesn't seem that harmful. Easy to get from the grocery store. I don't need a fast way to dissolve copper. And I would like not to use nitric or sulphuric. I am pretty sure I will need to use HCl for, the iron in the silverplated electrolysis method is abundant.
First I will apologize for coming out that hard in the beginning, human factors.
The intention still stand.
Anyway your idea of research and ours may differ as there are many threads in this forum discussing the same topic.
And unless you have read the ones on the topic to the end I do not consider it as the research has been done.
You can of course make a small test.
But it will create much more waste than HCl for example, and the waste created is as dangerous or even more as the Chlorides.
Acetates are as they come from an organic acid, more readily taken up by living things.
And all waste has to be treated.
Regarding to my request to who and what you are asking, is that we commonly get people asking questions which clearly refers to either a post a poster or both and do not quote the information to which they ask about.
Since most threads in here is live and winding back and forth in topic it is next to impossible to answer questions, unless the one asking has used the reply to button.