Yes, I saw a recommendation for Hazen Research. I will inquire tomorrow. Thank you so much! I am in Colorado, but I could send samples anywhere in the US. (If for some reason that one didn't work out.)It has been done as a reply to your question in another thread.
And of course your general location will make it easier to recommend someone.
And the pictures in the textbooks are way more detailed than most of the out of focused cellphone pictures posted here.
And you are right, good pictures accompanied by detailed information can have good value.
Rhodium ore is not a one thing.
Rhodium is a bi product of other PGMs mined, and I'm wondering if you mean Radium?
A totally different beast all together.
So is Rhodium just a refined product? Does it not occur naturally? I am just getting into the PGM's, and there is certainly a lot to learn.