Ok so i did research(not too extensivly im afraid) and i have already put my cbs, fingers, pins and mother boards in to AR here is what i have so far...
1 i placed everything into a pyrex jar and placed it on a heating plate and slowly poured the AR solution over the material
2 i let it sit until there was no more visible reactions occuring and then filtered the solution into another beaker...the solution was a pure black but i proceeded anyway
3 i poured an equal amount of water into the soluion and finally so uniodized table salt in order to pull any silver out of soluion, i decanted, filtered and baged the white substance in the filters and at the bottom of the jar which i believe to be silver cloride
4 next i poured into my leftover soluion some sodium sulfate, decanted and filtered the soluion and now im left with what looks like sand with some pepper in it, i believe this is gold sulfide , i dont know what is left in the solution and i dont know if what i have is actually gold or not but i havent throw away anything i just dont want my efforts of have been a waste
i got my information from various sources and from http://www.49ermike.com/aqua_regia_clean.shtml
1 i placed everything into a pyrex jar and placed it on a heating plate and slowly poured the AR solution over the material
2 i let it sit until there was no more visible reactions occuring and then filtered the solution into another beaker...the solution was a pure black but i proceeded anyway
3 i poured an equal amount of water into the soluion and finally so uniodized table salt in order to pull any silver out of soluion, i decanted, filtered and baged the white substance in the filters and at the bottom of the jar which i believe to be silver cloride
4 next i poured into my leftover soluion some sodium sulfate, decanted and filtered the soluion and now im left with what looks like sand with some pepper in it, i believe this is gold sulfide , i dont know what is left in the solution and i dont know if what i have is actually gold or not but i havent throw away anything i just dont want my efforts of have been a waste
i got my information from various sources and from http://www.49ermike.com/aqua_regia_clean.shtml