• Please join our new sister site dedicated to discussion of gold, silver, platinum, copper and palladium bar, coin, jewelry collecting/investing/storing/selling/buying. It would be greatly appreciated if you joined and help add a few new topics for new people to engage in.

    Bullion.Forum

Chemical Newbie

Gold Refining Forum

Help Support Gold Refining Forum:

This site may earn a commission from merchant affiliate links, including eBay, Amazon, and others.

ritehere

Well-known member
Joined
Feb 13, 2012
Messages
67
Just beginner here and had a question.
I desolved gold particals and fingers using the acid/clorox method like in the videos. But the solution that I got wasn't a deep goldish yellow it was a more tinted yellowish/green. Let it sit overnight and then used bms to try and drop gold. But the solution turned to clear and just stayed clear.
What could I have done wrong?
 
If there was gold in solution and nothing has dropped then you probably still have an excess of oxidiser (bleach in this case).
Heat the solution to drive off excess chlorine and then add more smb.
 