butcher said:
thanks for catalog can you tell us what those words mean,

:?:
The 7 columns of the table, from left to right:
type of parts ... Au ... Ag... Pt... Pd ... Ru... Ta
from page 1 to 58 are
IC's
58-105 are
diodes, transistors, thyristors, stabilitron ....
105-111 are
capacitors
111-136 are
resistors, potentiometers
136-175 are
conectors and switches
175-181 are
quartz resonator and filters, transformers, delay lines
181-191 are
tubes/valves(electronic tubes)
Here is some links:
http://www.rustran.com (or you can choose any translator)
and
http://www.google.ro/imgres?imgurl=http://linguistica.insite.com.br/images/russian-alphabet.gif&imgrefurl=http://linguistica.insite.com.br/cgi-bin/russian&h=842&w=484&sz=13&tbnid=qEks32h8ZI2JZM:&tbnh=145&tbnw=83&prev=/images%3Fq%3Drussian%2Balphabet&hl=ro&usg
I attached this catalog for Dimitry(he asked me), but I thought that might be useful for everybody -at least as a reference, to compare it with not/non Russian electronic parts-
of course, with a little(minimum) search job, and maybe with a little kindness....
In this catalog the numbers are more important than the words, for example when you realize that in 1000 pieces of connectors can be over 2 kg of gold...
...anyway If is not interesting for someone else too, then I can delete it.