diego Henrique vilela
Active member
Olá, boa noite, alguém poderia indicar um agente despoluente eficiente para paládio. Tenho fios de cobre banhados a paládio, preciso retirar o paládio sem destruir o fio de cobre.
Welcome to us.Olá, boa noite, alguém poderia indicar um agente despoluente eficiente para paládio. Tenho fios de cobre banhados a paládio, preciso retirar o paládio sem destruir o fio de cobre.
I’m not aware of any method that can do that.Remove Palladium
Hello, good evening, could anyone indicate an efficient depolluting agent for palladium. I have palladium-plated copper wires, I need to remove the palladium without destroying the copper wire.
If the plating is not too thick and you do not need the Copper wire.Remove Palladium
Hello, good evening, could anyone indicate an efficient depolluting agent for palladium. I have palladium-plated copper wires, I need to remove the palladium without destroying the copper wire.
In stead of replying to my question, you reported me??Remove Palladium
Hello, good evening, could anyone indicate an efficient depolluting agent for palladium. I have palladium-plated copper wires, I need to remove the palladium without destroying the copper wire.
sorry for my bad english. I went to the wrong place. I have 2 tons of these wires. every 1 kilo has 1 gram of palladium... therefore 2 kilos of Palladium. it's a lot of copper material to be attacked ... I need to develop a deplacing method. understand my situation?In stead of replying to my question, you reported me??
That is what you do if someone breaks the rules.
So I assume you did intend to reply.
And Nitric will dissolve both Palladium and Copper.
How much wire do you have?
You can dissolve all and then cement it back on Copper bus bars or similar.
Nitric is not a way of doing it as the Nitric will dissolve the Palladium as well.sorry for my bad english. I went to the wrong place. I have 2 tons of these wires. every 1 kilo has 1 gram of palladium... therefore 2 kilos of Palladium. it's a lot of copper material to be attacked ... I need to develop a deplacing method. understand my situation?
sorry for my bad english. I went to the wrong place. I have 2 tons of these wires. every 1 kilo has 1 gram of palladium... therefore 2 kilos of Palladium. it's a lot of copper material to be attacked ... I need to develop a deplacing method. understand my situation?
You suggested cementing with copper because it would only precipitate the palladium. correct ?In stead of replying to my question, you reported me??
That is what you do if someone breaks the rules.
So I assume you did intend to reply.
And Nitric will dissolve both Palladium and Copper.
How much wire do you have?
You can dissolve all and then cement it back on Copper bus bars or similar.
Yes, and when there is only Copper and Palladium in solution it will not bring any other "contaminants" into the mix.You suggested cementing with copper because it would only precipitate the palladium. correct ?
Interesting.A copper cell may be viable. I know very little about palladium so the sulfuric based electrolyte may or may not be a problem depending on where the palladium is left. Maybe in the slimes and maybe in the electrolyte. Just a thought on my part.
According to Wikipedia it is soluble in hot concentrated Sulfuric, which should make safe,A copper cell may be viable. I know very little about palladium so the sulfuric based electrolyte may or may not be a problem depending on where the palladium is left. Maybe in the slimes and maybe in the electrolyte. Just a thought on my part.
Thanks for all the suggestions I'm enjoying the forumAccording to Wikipedia it is soluble in hot concentrated Sulfuric, which should make safe,
with the "weak" cold Sulfuric in a copper cell.
According to Wikipedia it is soluble in hot concentrated Sulfuric, which should make safe,
with the "weak" cold Sulfuric in a copper cell.
I went to the wrong place. I have 2 tons of these wires. every 1 kilo has 1 gram of palladium... therefore 2 kilos of Palladium. it's a lot of copper material to be attacked
Olá, você tem grandes quantidades deste fio? refinamos e compramos paládio e todos os PGMsOlá, boa noite, alguém poderia indicar um agente despoluente eficiente para paládio. Tenho fios de cobre banhados a paládio, preciso retirar o paládio sem destruir o fio de cobre.