I still have a few of those put away. I use a few at times for cementing waste solutions.
It's gold through the board. I confirmed with the board room at my job. They design these boards.I'm still confused, I can't imagine that there is gold between the two surfaces, on the inside of the board. OP I think you need to cut one to confirm.
The only time I've ever seen gold anywhere other than on the surface is with fully plated vias and through-holes, and that's pretty rare. Even then it's still on the "outside" and can be recovered with Copper Chloride etching.
Yes but how? Photos would help, even if you think it's difficult to see we can recognize it.It's gold through the board. I confirmed with the board room at my job. They design these boards.
If it is internal to the boards all of the drawings in the world will not allow the chemistry to reach the internal spaces without mechanical destruction to expose it. So all of the explanations of how it is applied are moot without the application of a big hammer. (or hopefully a more efficient way of exposing the gold)Yes but how? Photos would help, even if you think it's difficult to see we can recognize it.
I think most likely these are just ENIG with open vias, and OP has interpreted "through the board" to mean there is gold inside somewhere, which I have never seen and I don't really believe exists. It's possible in theory with a multilayer board but OP says they are not multilayer. Also I don't think there would be much point in having gold internally as those layers are not subject to oxidation.If it is internal to the boards all of the drawings in the world will not allow the chemistry to reach the internal spaces without mechanical destruction to expose it. So all of the explanations of how it is applied are moot without the application of a big hammer. (or hopefully a more efficient way of exposing the gold)
Yes true, but according to the OP the boards are produced in house and single layer, double sided with through vias with Gold.If it is internal to the boards all of the drawings in the world will not allow the chemistry to reach the internal spaces without mechanical destruction to expose it. So all of the explanations of how it is applied are moot without the application of a big hammer. (or hopefully a more efficient way of exposing the gold)
OP didn't mention vias, that's what I'm trying to clarify- whether or not he believes there is gold in some internal layer which cannot be accessed. If it's just in the vias it can be easily got by Copper Chloride etching, unless they are epoxy-filled in which case I'd say it's not worth the effort of going after such a small amount.Yes true, but according to the OP the boards are produced in house and single layer, double sided with through vias with Gold.
And since he has been talking directly to the designers I'm inclined to believe his description.
This is a situation where direct leaching would suffice and no crushing should be necessary.
Pictures would be nice but the description is relatively clear.
Here is what he said:OP didn't mention vias, that's what I'm trying to clarify- whether or not he believes there is gold in some internal layer which cannot be accessed. If it's just in the vias it can be easily got by Copper Chloride etching, unless they are epoxy-filled in which case I'd say it's not worth the effort of going after such a small amount.
And then:They come from my job. I work on automated welding machines. I asked the guy who designs our PCB boards, and he did confirm that gold goes through the board. Some of these boards are having high frequency/temps/current going through. So, I believe that is why the boards were designed and made this way.
Sorry for the not so good description. It is a single layer boards. But, the traces run in both sides of the board and they follow all the way through the depth of the board. If I could get a good pic I would send it. But, it is so hard to see. I confirmed with the guy in our board room and the gold traces do run through the board. All be it very thin traces.
Yes me neither, because we are assuming that it goes through the board by conventional means, ie with vias. If so then there should be no need to shred the board as it's not internal. The title of the post suggests otherwise, but I think that is an error.As far as I'm concerned, I can't come up with another way of interpret it.
I'm still confused, I can't imagine that there is gold between the two surfaces, on the inside of the board. OP I think you need to cut one to confirm.
The only time I've ever seen gold anywhere other than on the surface is with fully plated vias and through-holes, and that's pretty rare. Even then it's still on the "outside" and can be recovered with Copper Chloride etching.
Ok well the focus is not great, can't quite tell if it's a multilayer board, but yes those are vias. They may be gold plated or possibly gold filled.Here is a picture that some people was asking for. Hopefully this clears some stuff up!!!
The focus is actually really good for how small those traces are. It's not a multi layered board. Those traces just run through it and stops at the point where you are supposed to add a component. They are not very big at all, nor are they that long.Ok well the focus is not great, can't quite tell if it's a multilayer board, but yes those are vias. They may be gold plated or possibly gold filled.
How many of these boards do you have? If its not too many, you could try drilling the vias out with a small drill bit and collecting the swarf to process.
If it is a multilayer board and you believe the internal layers have gold plated traces, they will need to be shredded.
It looks like it has quite a thick solder mask, I think I would use lye to remove that first, then it would be easier to see where the gold is and decide what to do next. If the vias are open (with a hole going all the way through) then you can just use a normal Copper Chloride etch without shredding the boards.The focus is actually really good for how small those traces are. It's not a multi layered board. Those traces just run through it and stops at the point where you are supposed to add a component. They are not very big at all, nor are they that long.