"Quadratic precipitant" (Shor) sounds like an interesting alternative to metabisulfite for dropping gold, but a search of the forum reveals no mention of it. Has anyone here used it? Know anything about it, good or bad?
 
Lelander said:
"Quadratic precipitant" (Shor) sounds like an interesting alternative to metabisulfite for dropping gold, but a search of the forum reveals no mention of it. Has anyone here used it? Know anything about it, good or bad?

Just say NO. Just search Shor.
 
I used it and also liked it. Order more from shor and been waiting just about a month on it. I had a response from two inquiries from them about a week apart and then radio silence. Nothing for last two weeks! Requested refund or just a response period and nothing... f*uc% shor
 
I used it and also liked it. Order more from shor and been waiting just about a month on it. I had a response from two inquiries from them about a week apart and then radio silence. Nothing for last two weeks! Requested refund or just a response period and nothing... f*uc% shor
The quadratic precipitantvis just SMB or a similar Sulfite.
 
This stuff is ridiculously expensive and doesn’t work as they say it does. However, when mixed with sodium metabisulfite it works great.
 