Hi, I just did a cat with poor man's ar. When I added soda
Ash to bring the ph up a foam formed that wouldn't go away
And after 7 tsp the ph is still 2. Does the ph + that lasersteve
Used on the DVD work better? Can I add 50-100% water to
The acid to aid in the ph increase without making the acid too
Weak to dissolve the zinc?
Thanks,
Steve