mythen10
Well-known member
- Joined
- Jun 25, 2022
- Messages
- 259
Hi I have a question, i wanna dissolve some relay contacts (silver palladium alloy) in nitric acid . My question is next : to recover silver and palladium is good to drop first silver from solution with sodium chloride dissolved in little water and after check the solution for platinum with ammonium chloride and in final after filtration of silver chloride and platinum if is present to put in solution some concentrated HCl acid to make aqua regia and after neutralise the nitric with urea and in the final step to add aluminium ? IT IS GOOD TO RECOVER THE PALLADIUM IN THIS WAY WITH ALLUMINIUM?(I don't have acces to zinc and dimerhylglioxime) THE PALLADIUM WILL DROP WITH ALLUMINIUM?