I collected everything and redefined again late last night ended up dropping about .6 gold which has been dried and added to jar. I found out that the solution in the vase was changed to another vase by my wife and it was never rinsed until before it went in the stockpot...... I know I know...... although I did get something at precipitated out after putting copper into the solution after drop. It is kind of a light pink precipitant which kind of makes me think platinum group metals I will attach a picture and set aside, I'm not ready to start with platinum yet. I'm good with silver and learning gold more and more, platinum groups are a different story