Okay sir i will try thisIf it dissolves completely in Nitric it is NOT Gold.
If there are some powder left it may be some Gold.
Filter it well and see if there is something black in the filter paper.
Okay sir i will try thisIf it dissolves completely in Nitric it is NOT Gold.
If there are some powder left it may be some Gold.
Filter it well and see if there is something black in the filter paper.
I check in xrf the gold was show in xrf testing not before buy check now i check all dust powder in xrf the gold was show 50 60 percent and i put some dust in nitric end the end black powder is remaing now black powder was not dissolving in nitricGood morning to all of You guys
Have a Bless day.
Sometimes it has been seen that some peoples or some web sites, sell a supposed gold powder.
The seller puts a little bit of gold powder.
very minimum ,Just enough so that the xrf machines can read that small amount of gold powder.
But in reality everything they sell you is not gold.